Abstract
The growing characteristics of metallic iron particles during reductive roasting of boron-bearing magnetite concentrate under different conditions were investigated. The size of the metallic iron particles was quantitatively measured via optical image analysis with consideration of size calibration and weighted ratio of image numbers in the core, middle and periphery zones of cross-section of pellets. In order to guarantee the measurement accuracy 54 images were captured in total for each specimen, with a weighted ratio of 1:7:19 with respect to the core, middle and periphery section of the cross-section of pellets. Increasing reduction temperature and time is favorable to the growth of metallic iron particles. Based on the modification of particle size measurement, in terms of time (t) and temperature (T) a predicting model of metallic iron particle size (D), was established as: D=125-0.112t-0.2352T-5.355×10-4t2+2.032× 10-4tT +1.134×10-4T2.
摘要
研究了不同还原条件下含硼铁精矿在焙烧过程中金属铁颗粒的生长规律. 采用光学显微镜获取还原球团的数字图像, 考虑到球团不同部位金属铁颗粒生长情况的差异, 采用回归拟合分析得到内、 中、 外区域的权重比例为 1:7:19, 每个样品根据此权重比例共获取 54 张图像. 基于修正后的金属铁颗粒尺寸的测定方法, 建立了铁颗粒平均粒径D (μm)与还原温度 T (°C)、 时间 t (min)之间的回归模型: D=125−0.112t−0.2352T−5.355×10−4t2+2.032×10−4tT+1.134×10−4T2.
Article PDF
Similar content being viewed by others
Avoid common mistakes on your manuscript.
References
GAO P, YU J W, HAN Y X, ZHOU M G. Mineralogical study of boron-bearing iron concentrate ore [J]. Journal of Northeastern University, 2015, 36(4): 581–584. DOI: 10.3969/j.issn.1005-3026. 2015.04. 027. (in Chinese)
LIU R, XUE X X, LIU X, WANG D S, FENG C, HUANG D W. Progress on China's boron resource and the current situation of boron-bearing materials [J]. Bulletin of the Chinese Ceramic Society, 2006, 25(6): 102–107. DOI: 10.16552/j.cnki.issn1001-1625.2006.06.025. (in Chinese)
ZHAO Q J, WANG C R, WANG C R, LIAN X Q. New process of multipurpose utilization of ludwigte [J]. Journal of Northeastern University (Natural Science), 1996, 17(6): 588–592. DOI: http://www.cnki.com.cn/Article/CJFDTotal-DBDX606.002.htm. (in Chinese)
CAO Z, CAO Y D, GUI F. Research status and progress of the exploitation and utilization of Paigeite ore [J]. Multipurpose Utilization of Mineral Resources, 2013(2): 17–20. DOI:10.3969/j.issn.1000-6532.2013.02.005. (in Chinese)
WANG G, XUE Q G, WANG J S. Carbothermic reduction characteristics of ludwigite and boron-iron magnetic separation [J]. International Journal of Minerals Metallurgy and Materials, 2018, 25(9): 1000–1009. DOI: 10.1007/s12613-018-1650-3.
WANG Guang, WANG Jing-song, XUE Qing-guo. Properties of boron-rich slag separated from boron-bearing iron concentrate [J]. Journal of Central South University, 2018, 25: 783–794. DOI: 10.1007/s11771-018-3783-y.
ZHANG X, LI G H, YOU J X, WANG J, LUO J, DUAN J, ZHANG T, PENG Z W, RAO M J, JIANG T. Extraction of boron from ludwigite ore: Mechanism on soda-ash roasting of Lizardite and Szaibelyite [J]. Minerals, 2019, 2019(9): 533. DOI: https://doi.org/10.3390/min9090533.
LIU G S, STREZOV V, LUCAS J A, WIBBERLEY L J. Thermal investigations of direct iron ore reduction with coal [J]. Thermochimica Acta, 2004, 410(1, 2): 133–140. DOI: 10.1016/s0040-6031(03)00398-8.
PARISI D R, LABORDE M A. Modeling of counter current moving bed gas-solid reactor used in direct reduction of iron ore [J]. Chemical Engineering Journal, 2004, 104(1-3): 35–43. DOI: 10.1016/j.cej.2004.08.001.
RAO M, LI G, ZHANG X, LUO J, PENG Z, JIANG T. Reductive roasting of nickel laterite ore with sodium sulfate for Fe-Ni production. Part I: Reduction/sulfidation characteristics [J]. Separation Science and Technology, 2016, 51(8): 1408–1420. DOI:10.1080/01496395.2016.1162173.
LI G, YOU Z, ZHANG Y, RAO M, WEN P, GUO Y, JIANG T. Synchronous volatilization of Sn, Zn, and As, and preparation of direct reduction iron (DRI) from a complex iron concentrate via CO reduction [J]. JOM Journal of the Minerals Metals and Materials Society, 2014, 66(9): 1701–1710. DOI: 10.1007/s11837-013-0852-4.
AL-THYABAT S, MILES N J. An improved estimation of size distribution from particle profile measurements [J]. Powder Technology, 2006, 166(3): 152–160. DOI: 10.1016/j.powtec.2006.05.008.
DONSKOI E, SUTHERS S P, FRADD S B, YOUNG J M, CAMPBELL J J, RAYNLYN T D, CLOUT J M F. Utilization of optical image analysis and automatic texture classification for iron ore particle characterisation [J]. Minerals Engineering, 2007, 20(5): 461–471. DOI: 10.1016/j.mineng.2006.12.005.
HUKKANEN E J, BRAATZ R D. Measurement of particle size distribution in suspension polymerization using in situ laser backscattering [J]. Sensors and Actuators B-Chemical, 2003, 96(1, 2): 451–459. DOI: 10.1016/s0925-4005(03)00600-2.
KOH T K, MILES N J, MORGAN S P, HAYES- GILL B R. Improving particle size measurement using multi-flash imaging [J]. Minerals Engineering, 2009, 22(6): 537–543. DOI: 10.1016/j.mineng.2008.12.005.
SUN Y, HAN Y, GAO P, YU J. Size distribution behavior of metallic iron particles in coal-based reduction products of an oolitic iron ore [J]. Mineral Processing and Extractive Metallurgy Review, 2015, 36(4): 249–257. DOI: 10.1080/08827508.2014.955611.
MAITI A, CHAKRAVARTY D, BISWAS K, HALDER A. Development of a mass model in estimating weight-wise particle size distribution using digital image processing [J]. International Journal of Mining Science and Technology, 2017, 27(3): 435–443. DOI: 10.1016/j.ijmst.2017.03.015.
DONSKOI E, RAYNLYN T D, POLIAKOV A. Image analysis estimation of iron ore particle segregation in epoxy blocks [J]. Minerals Engineering, 2018, 120: 102–109. DOI: 10.1016/j.mineng.2018.02.024.
LUO L, ZHANG H. Process mineralogy and characteristic associations of iron and phosphorus-based minerals on oolitic hematite [J]. Journal of Central South University, 2017, 24(9): 1959–1967. DOI:10.1007/s11771-017-3604-8.
LI G, LIANG B, RAO M, ZHANG Y, JIANG T. An innovative process for extracting boron and simultaneous recovering metallic iron from ludwigite ore [J]. Minerals Engineering, 2014, 56: 57–60. DOI: 10.1016/j.mineng. 2013.10.030.
LIANG B, LI G, RAO M, PENG Z, ZHANG Y, JIANG T. Water leaching of boron from soda-ash-activated ludwigite ore [J]. Hydrometallurgy, 2017, 167: 101–106. DOI: 10.1016/j.hydromet.2016.11.004.
LI G, FANG L, ZHANG X, LIANG B, RAO M, PENG Z, JIANG T. Utilization of the MgO-rich residue originated from Ludwigite ore: Hydrothermal synthesis of MHSH whiskers [J]. Minerals, 2017, 7(8): 138–145. DOI: 10.3390/min7080138.
CHAYES F. On the bias of grain-size measurements made in thin section [J]. Journal of Geology, 1950, 58(2): 156–160. DOI: 10.1086/625716.
CUZZI J N, OLSON D M. Recovering 3D particle size distributions from 2D sections [J]. Meteoritics & Planetary Science, 2016, 52(3): 532–545. DOI:10.1111/maps.12812.
NAPPER D H. Particle growth in suspensions [J]. Journal of Colloid & Interface Science, 1974, 46(1): DOI: 10.1016/0021-9797(74)90040-X.
SUN Y S, HAN Y X, LI Y F, LI Y J. Formation and characterization of metallic iron grains in coal-based reduction of oolitic iron ore [J]. International Journal of Minerals Metallurgy & Materials, 2017, 24(2): 123–129. DOI: 10.1007/s12613-017-1386-5.
Author information
Authors and Affiliations
Corresponding author
Additional information
Foundation item: Project(51804346) supported by the National Natural Science Foundation of China; Project(2019JJ50767) supported by the Natural Science Foundation of Hunan Province, China; Project(KY [2017]125) supported by Youth Foundation of Guizhou Education Department, China
Rights and permissions
About this article
Cite this article
Zhang, X., Li, Gh., Rao, Mj. et al. Growth of metallic iron particles during reductive roasting of boron-bearing magnetite concentrate. J. Cent. South Univ. 27, 1484–1494 (2020). https://doi.org/10.1007/s11771-020-4384-0
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11771-020-4384-0