Abstract
Material degradation due to unidirectional sliding wear can be found in wide range of engineering applications. Depending on the applied load and sliding velocity, several material removal mechanisms will be operative during sliding. Lim and Ashby compile these mechanisms in the form of wear mechanism map. They have also been able to estimate the wear rate in each mechanism quantitatively. However, no effort has hitherto been made to use these expressions and concepts to alter or modify the surfaces of various materials for improved wear performances. The objective of the present work is to address this issue. In this work, the expression for wear rate in various regimes will be examined critically. The important parameters that governs wear rate will be identified. An approach to improve wear rate in each regime will be suggested on the basis of identified parameters. Suggestions will be substantiated with large database and published work.
Article PDF
Similar content being viewed by others
Avoid common mistakes on your manuscript.
References
Lim S C and Ashby M F, Acta Met, 35 (1987) 11
Blomerg A, Olsson M and Hogmark S, Wear, 171 (1994) 77
Roy M, Ray K K and Sundararajan G, Metal. And Mater. Trans., 32A (2001) 1431.
Hirst W and Lancaster J K, J. Appl. Phys. 27 (1956) 1057.
Hogmark S, Jacobson S and Larsson M, Wear, 246 (2000)20
Bunshah R F, Handbook of deposition techniques for films and Coatings, (2nd ed.) Noyes Publications, West wood, New Jersey, USA.
Wei Q and Narayan J, Int. Mater. Review, 45 (200) 133.
Veprek S, Thin Solid Films, 317 (1998) 449.
Wear Control Handbook, Eds. Peterson M B and Winer W O, New York, (1980).
Fundamentals of Friction and Wear, Ed. Regney D.A., Metals Park, Ohio, ASM, (1981).
Ahmed R and Hadfield M, Wear, 230 (1990) 39
Roy M, Ch. V Subha Rao, Rao D S and Sundararajan G, Surface Engineering, 15 (1999) 129
Bozzi A C and B de Mello J D, Wear, 233–235 (1999) 575
Yinglong W, Yuansheng J and Shizhu W, Wear, 128 (1988) 265
Roy M and Sundararajan G, Proc. 12th Int. Tribol. Colloquium, Jan, 2000 Stuttgart, Germany, p-1971.
Garg D and Dyer P N, Wear, 162–164 (1993) 552
Voyer J and Marple B R, Wear, 225–229 (1999) 135
Roy M, Narkhede B E and Paul S N, Proc. Int. Conf. On Industrial Tribol. Dec., 1999 Hyderabad, India, p-215.
Wood R J K, Meller B J and Binfield M L, Wear, 211 (1997) 70.
Bahadur S and Yang C N, Wear 196 (1996) 156.
Lin P, Deshpandey C, Doerr H J, Bunshah R F, Chopra K L and Vankar V D, Thin Solid Films, 153 (1987) 487.
Lee K S, Kim Y S, Tosa M, Kasahara A and Yosihara K, Appl. Surf. Sci., 169–170 (2001) 420.
Holmberg K and Matthews A, Coatings Tribology, Tribology Series, 28, Elsevier, Amsterdam, (1994).
Hiroven J P, Koskien J, Jervis J R and Natasi M, Surf. Coat. Technol., 80 (1996) 139.
Hogmark S, Hollman P, Alahelisten A, Hedenqvist P, Wear, 200 (1996) 225.
Krishnaraj N, Iyer K J L, Sundaresan S, Wear 210 (1997)237
Rizvi S A and Khan T I, Tribol. Intl., 32 (1999) 567.
Budinski K G, Wear, 162–164 (1993) 757.
Wang A G and Hutchings I M, Wear, 124 (1988)149.
Gordienko A I, Ivaskko V V and Bushik S V, Phy. and Chem. of Materials Treatment, 23 (1989) 208.
Tananko I A, Levchenko A A, Guiva R T, Guiva V A and Sitsevaya E Yu, Phy. and Chem. of Materials Treatment, 25 (1991) 529.
Sundararajan G, Scripta. Metal, 32 (1995) 523.
Fu Y, Batchelor A W and Loh N L, Wear, 218 (1998) 250.
Dingremont N, Bergmann E and Collignon P, Surf. Coat. Technol. 72(3) (1995) 157.
Dingremont N, Bergmann E, Collignon P and Michel H, Surf. Coat. Technol., 72(3) (1995)163
Johansson E, Surface modification in tribology, Acta Universitatis Upaliensis Dissertation in Science and Technology, Vol433,1993.ISBN 91-554-3061-6, Paper VII.
Jia K and Fischer T E, Wear, 200 (1996) 206
Wang Y, Jiang S, Wang M and Wang S, Xiao T.D. and Strutt P.R., Wear, 237 (2000) 176.
Roy M, Pauschitz A, Pollak R and Franek F, Tribology Int. 39 (2006) 29.
Rebholz C, Leyland A, larour P, Choritidis C, Logotletidis S, and Matthews A, Surf. Coat. Technol., 116–119 (1999) 648.
Rebholz C, Leyland A, Schneider D, Schuttrich B, Charitidis C, Logothetidis S and Mathews A., Thin Solid Films (in Press)
Rebholz C, Schneider J M, Logotletidis S, Matthews A.. Surf. Coat. Technol. 112 (1999) 85
Quin T F J, Sullivan J L and Rowson D M, Wear, 94 (1984)175.
Rowson D M and Quinn T F J, J. Phy. D. Appl. Phys., 13 (1980) 209
Quin T F J, Wear, 216 (1998) 262–275.
Malgaord J and Srivastaba V K, Wear, 41 (1977) 263.
Roy M, Ray K K and Sundararajan G, Oxid. Metals, 50 (1999)
Kubaschewski O and Hopkins B E, Oxidation of Metals and Alloys, Buttersworth London, (1962).
Hirose A, Ueda T and Kobayashi K F, Mater. Sci.and Engg. 160A (1993) 143.
Tau Y H and Doong J L, Wear, 132 (1989) 9.
Gawne D T and MA U, Wear, 129 (1989) 123.
Schmutzler H J, Viefhaus H and Grabke H -J, Surf. Interface Anal., 18 (1992) 581.
Dankov P D and Churuev P V, C.R. Acad. Sci. U.R.S.S., 73 (1950) 1221
Peters F and Engell H J, Arch, Eisenhullenw
Cox B, Progr. Nad. Energy Ser, 4 (1961) 166
Smeltzer W W, Acta Met., 8 (1960) 268
Moreau J and Cognet M, Rev. Metall, 55 (1958) 1091.
Pilling N B and Bedworth R E, J. Inst. Met., 29 (1923) 529
Engell H J, Werkstoffe, Korrosion, 11 (1960) 147.
Hou P Y and Stringer J, Oxid. Met., 38 (1992) 323.
Sigler D R, Oxid. Met., 40 (1993) 555.
Bennett M J and Haulton P, ’High Temperature Materials for Power Engineering; (ed. E. Bachelet) 189, 1990, Dorlrecht, Kluwer, Academic Publishers.
Tatlock G J and Hard T J, Oxid. Met., 22 (1984) 201.
Gobel M, Rahmel A and Schertzc M, Oxid. Met., 3–4 (1993) 231
Sun J H, Jang H C and Chang E, Surf. Coat. Technol., 64 (1994)195
Vernon-Perry K D, Crovenor C R M, Needhan N. and English T, Mater. Sci. Technol., 4 (1988) 461
Pint B A, Oxid. Met., 48 (1997) 303
Ramnarayanan T A, Raghavan M and Petkvichuton R, J. Electrochem. Soc., 131 (1984) 923.
Forest C and Davidson J H, Oxid. Metals, 43 (1995) 479.
Wang Y, Kovacevic R, Lia J, Wear, 221 (1998) 47–53.
Giggin C S and Pettit F S, Met. Trans., 2 (1971) 1071
Wood G C and Stott F H, Mater. Sci. and Technol, 3 (1987) 517
Whittle D P and Stringer J, Phil. Trans. R. Soc. (London) 295A (1980) 304
Roy M, Pauschitz A and Franek F, Tribologie und Schmierungstechnik, 50 (2003) 40.
Fountain J G., Golightly F A, Scott F H and Wood G C, Oxid. Met., 10 (1976) 341
Allan I M, Akuezue H C and Whittle D P, Oxid. Met., 14 (1980) 517
Wells A and Dewet D J, Wear, 127 (1988) 269
Eylon D and Belts R K and Fujishro S, Thin Solid Films, 73 (1980) 323.
Metals Reference Book, e.d. Smithels C.J.. Butterworths. London & Boston, 5th ed. 1976.
Wei J and Xue Q, Wear, 162–164 (1993) 229.
Barbezat G, Nicoll A R and Sickinger A, Wear, 162–164 (1993) 529–537.
Roy M, Pauschitz A and Franek F, Proc. Int. Corrosion Congress. Sept., 2002, Granada, Spain.
Hsu M J and Molians P A, Wear, 132 (1989) 123
Okado J, Shima M, Mccoll I R, Watertions R B, Osegava T H and Kasaya M, Wear, 225–229 (1999) 749.
Stachowiak G W, Stachowiak G D and Batchelor A W, Wear 178 (1994) 69.
Sawyer W G and Blanchal T A, Wear, 225–229 (1994) 581.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Roy, M. Use of wear mechanism map to engineer surfaces for enhanced wear resistance. Trans Indian Inst Met 62, 197–208 (2009). https://doi.org/10.1007/s12666-009-0032-y
Received:
Revised:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s12666-009-0032-y