Conclusions
Investigations were made of existing methods of drying of the monolithic linings of the steel teeming ladles of the open hearth shops of Nizhnii Tagil and Magnitogorsk Metallurgical Combines and their shortcomings were revealed.
A burner was developed providing more uniform heating of the ladle lining and permitting drying using any specified cycle.
A significant saving in fuel and a reduction in drying time were obtained.
Article PDF
Similar content being viewed by others
Avoid common mistakes on your manuscript.
Literature cited
P. P. Lutsik, B. P. Dromenko, I. P. Tsibin, et al., Ogneupory, No. 4, pp. 48–52 (1985).
V. A. Samsonov, A. A. Sharaev, E. S. Cherdantseva, et al., Metallurg, No. 5, 25–26 (1984).
V. A. Samsonov, A. A. Sharaev, A. V. Marchenko, and V. N. Antonov, Ogneupory, No. 2, 44–47 (1984).
Author information
Authors and Affiliations
Additional information
Translated from Ogneupory, No. 11, pp. 3–6, November, 1988.
Rights and permissions
About this article
Cite this article
Levchenko, Y.A., Strekotin, V.V., Bespamyatnykh, V.I. et al. Drying of steel teeming ladle monolithic linings. Refractories 29, 653–657 (1988). https://doi.org/10.1007/BF01280328
Issue Date:
DOI: https://doi.org/10.1007/BF01280328