The biomagnesium alloys have been considered to be one of the most potential biodegradable metal materials due to its good mechanical compatibility, biological compatibility, biological security and biodegradable characteristics. However, the two major problems of high degradation rates in physiological environment and low mechanical properties prevent the development of biomagnesium alloys. In the present work, the samples of Mg-Zn-Y-Nd alloy were prepared by cyclic extrusion compression (CEC) and equal channel angular pressing (ECAP). The microstructures, mechanical properties of alloy and its corrosion behavior in simulated body fluid (SBF) were evaluated. The results reveal that Mg-Zn-Y-Nd alloy consists of equiaxial fine grain structure with the homogeneous distribution of micrometer size and nano-sized second phase, which was caused by the dynamic recrystallization during the ECAP and CEC. The corrosion resistance of alloy was improved. The tensile and corrosion resistance were improved, especially the processed alloy exhibit uniform corrosion performances and decreased corrosion rate. This will provide theoretical ground for Mg-Zn-Y-Nd alloy as vascular stent application.
Article PDF
Similar content being viewed by others
Avoid common mistakes on your manuscript.
References
Wen Z H, Wu C J, Dai C S, et al. Corrosion behaviors of Mg and its alloys with different Al contents in a modified simulated body fluid. Journal of Alloys and Compounds, 2009, 488(1): 392–399
Witte F, Hort N, Vogt C, et al. Degradable biomaterials based on magnesium corrosion. Current Opinion in Solid State and Materials Science, 2008, 12(5–6): 63–72
Zhang S, Zhang X, Zhao C, et al. Research on an Mg-Zn alloy as a degradable biomaterial. Acta Biomaterialia, 2010, 6(2): 626–640
Gu X N, Zhou W R, Zheng Y F, et al. Degradation and cytotoxicity of lotus-type porous pure magnesium as potential tissue engineering scaffold material. Materials Letters, 2010, 64(17): 1871–1874
Li Z, Gu X, Lou S, et al. The development of binary Mg-Ca alloys for use as biodegradable materials within bone. Biomaterials, 2008, 29(10): 1329–1344
Hamu G B, Eliezer D, Wagner L. The relation between severe plastic deformation microstructure and corrosion behavior of AZ31 magnesium alloy. Journal of Alloys and Compounds, 2009, 468(1–2): 222–229
Yamashita A, Horita Z, Langdon T G. Improving the mechanical properties of magnesium and a magnesium alloy through severe plastic deformation. Materials Science and Engineering A, 2001, 300(1–2): 142–147
Alvarez-Lopez M, Pereda M D, del Valle J A, et al. Corrosion behaviour of AZ31 magnesium alloy with different grain sizes in simulated biological fluids. Acta Biomaterialia, 2010, 6(5): 1763–1771
Xia K, Wang J T, Wu X, et al. Equal channel angular pressing of magnesium alloy AZ31. Materials Science and Engineering A, 2005, 410–411(S1): 324–327
Jin L, Jin D L, Mao D L, et al. Microstructure evolution of AZ31 Mg alloy during equal channel angular extrusion. Materials Science and Engineering A, 2006, 423(1–2): 247–252
Song G L, Xu Z. Effect of microstructure evolution on corrosion of different crystal surfaces of AZ31 Mg alloy in a chloride containing solution. Corrosion Science, 2012, 54: 97–105
Estrin Y, Vinogradov A. Extreme grain refinement by severe plastic deformation: A wealth of challenging science. Acta Materialia, 2013, 61(3): 782–817
Gao J H, Guan S K, Ren Z W, et al. Homogeneous corrosion of high pressure torsion treated Mg-Zn-Ca alloy in simulated body fluid. Materials Letters, 2011, 65(4): 691–693
Gu X N, Li N, Zheng Y F, et al. In vitro study on equal channel angular pressing AZ31 magnesium alloy with and without back pressure. Materials Science and Engineering B, 2011, 176(20): 1802–1806
Wu Q, Zhu S, Wang L, et al. The microstructure and properties of cyclic extrusion compression treated Mg-Zn-Y-Nd alloy for vascular stent application. Journal of the Mechanical Behavior of Biomedical Materials, 2012, 8: 1–7
Song G L. Effect of texture on the corrosion behavior of AZ31 Mg Alloy. JOM, 2012, 64(6): 671–679
Lin J B, Wang Q D, Peng L M, et al. Microstructure and high tensile ductility of ZK60 magnesium alloy processed by cyclic extrusion and compression. Journal of Alloys and Compounds, 2009, 476(1–2): 441–445
Segal V M. Equal channel angular extrusion: from macromechanics to structure formation. Materials Science and Engineering A, 1999, 271(1–2): 322–333
Kokubo T, Takadama H. How useful is SBF in predicting in vivo bone bioactivity? Biomaterials, 2006, 27(15): 2907–2915
Song G L, Atrens A. Understanding magnesium corrosion — A framework for improved alloy performance. Advanced Engineering Materials, 2003, 5(12): 837–858
Jiang L, Jonas J J, Luo A A, et al. Influence of \(\{ 10\bar 12\}\) extension twinning on the flow behavior of AZ31 Mg alloy. Materials Science and Engineering A, 2007, 445–446: 302–309
Bohlen J, Yi S B, Swiostek J, et al. Microstructure and texture development during hydrostatic extrusion of magnesium alloy AZ31. Scripta Materialia, 2005, 53(2): 259–264
Zhang X B, Yuan G Y, Mao L, et al. Effects of extrusion and heat treatment on the mechanical properties and biocorrosion behaviors of an Mg-Nd-Zn-Zr alloy. Journal of the Mechanical Behavior of Biomedical Materials, 2012, 7(SI): 77–86
Author information
Authors and Affiliations
Corresponding authors
Rights and permissions
About this article
Cite this article
Zhu, SJ., Liu, Q., Qian, YF. et al. Effect of different processings on mechanical property and corrosion behavior in simulated body fluid of Mg-Zn-Y-Nd alloy for cardiovascular stent application. Front. Mater. Sci. 8, 256–263 (2014). https://doi.org/10.1007/s11706-014-0259-3
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11706-014-0259-3