This work investigates the response of porous carbonate building stones to acid deposition during a short-terra exposure period and the characteristics that influence their reactivity and/or durability. Several carbonate porous stones used in Spanish and English monuments were exposed to English urban and suburban environments. In each location they were both exposed to and sheltered from rainfall. Monthly analyses were carried out in order to investigate any possible sign of reaction. In addition, some physical properties of the stones relating to transfer of moisture were determined. Results indicate that the reactivity of these stones is relatively high, significant signs of reaction were detected within only a few months of exposure. Under the same environmental conditions, the response and reactivity of porous carbonate stones are determined by their petrophysical characteristics.
Article PDF
Similar content being viewed by others
Avoid common mistakes on your manuscript.
References
Butlin, R.N., Cooke, R.U., Jaynes, S.M. and Sharp: 1985,V th International Congress on Deterioration and Conservation of Stone, Press Polytechniques Romandes, Lausanne, 537–546.
Butlin, R.N., Yates, T.J.S., Coote, A.T, Lloyd, G.O. and Massey, S.W.:1993:The first phase of the National Exposure Programme, 1987–1991,Report. CR 253/93 Building Res. Establishment, Watford, 70 pages.
Cooke, R.U. and Gibbs, G.B.: 1993,Crumbling Heritage? Studies on Stone weathering in polluted atmospheres, National Power plc, Swindon, 68 pages.
Girardet, F. and Connor, M.:1992,Analusis Magazine,20, n.5, M26-M32.
Goturk, H., Volkan, M. and Kahveci, S.: 1993,Conserv. of Stone and Other Materials,1, E&FN SPON, 83–90
Grossi, C.M., Esbert, R.M.; Lewry, A.J. and Butlin, R.N.: 1994,Seventh International Congress International Association of Engineering Geology, A.A. Balkema, Rotterdam, 3573–3582.
Jaynes, S.M. and Cooke, R.U: 1987,Atmos. Environ. 21, 1601–1622
Johansson, L.G., Lindqvist, O and Mangio, R.E.: 1988,Durability of Building Materials,5, 439–449.
Lipfert, F.W.: 1989:Atmos. Environ. 23, 415–429.
Livingstone, R.A. 1992,7 th Int. Cong. on Deterioration and Conservation of Stone, LNEC, Lisbon, 375–386.
NAPAP, 1991:Effects of acidic deposition on materiah. National Acid Precipitation Assessment Program, Office of the Director of Research, Washington., D.C, 280 pages.
Spedding, D.J.: 1969:Atmos. Environ.,3, 683.
Spiker, E.C., Comer, V.J., Hosker, R.P. and Sherwood, S.I.: 1992,7 th Int. Cong. on Deterioration and Conservation of Stone, Labóratorio Nacional de Engenharia Civil, Lisbon, 641–650.
Webb, A.H, Bawden, R.J., Busby, A.K and Hopkins, J.N.: 1992,Atmos. Eviron.,26B, 165–181.
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Grossi, C.M., Murray, M. & Butlin, R.N. Response of porous building stones to acid deposition. Water Air Soil Pollut 85, 2713–2718 (1995). https://doi.org/10.1007/BF01186244
Issue Date:
DOI: https://doi.org/10.1007/BF01186244