Despite the advances in studies utilizing industrial, construction and agricultural wastes as alternative materials for concrete making, there are still gaps to be covered on the durability characteristics of most materials. This study presents a shot overview on the durability properties of alkali-activated slag (AAS) composites. The durability properties of AAS explored include permeability, alkali silica reaction, carbonation, freeze and thaw, fire resistance, corrosion, and resistance to sulphate, chloride and acid attacks. The research outcomes indicated that AAS possessed strong durability characteristics in terms of resistance to acid and sulphate attacks, however, areas such as permeability, alkali silica reaction, carbonation and freeze-thaw resistance, have not been overly explored. A general overview of the performance and limitations of AAS has been provided, and the study suggested specific areas for further investigations. The information provided in this study will be useful for users of AAS, and pave way for innovative researches on AAS composite.
Article PDF
Explore related subjects
Discover the latest articles, news and stories from top researchers in related subjects.Avoid common mistakes on your manuscript.
Change history
08 April 2020
The original version of this paper was unfortunately published as a book review, when it is a review article.
References
Said AM, Zeidan MS, Bassuoni MT, Tian Y (2012) Properties of concrete incorporating nano-silica. Constr Build Mater 36:838–844. https://doi.org/10.1016/j.conbuildmat.2012.06.044
Awoyera PO, Dawson AR, Thom NH, Akinmusuru JO (2017) Suitability of mortars produced using laterite and ceramic wastes: mechanical and microscale analysis. Constr Build Mater 148:195–203. https://doi.org/10.1016/j.conbuildmat.2017.05.031
Awoyera PO, Akinmusuru JO, Ndambuki JM (2016) Green concrete production with ceramic wastes and laterite. Constr Build Mater 117:29–36. https://doi.org/10.1016/j.conbuildmat.2016.04.108
Netinger I, Bjegović D, Vrhovac G (2011) Utilisation of steel slag as an aggregate in concrete. Mater Struct 44:1565–1575. https://doi.org/10.1617/s11527-011-9719-8
Karthik S, Rao PRM, Awoyera PO (2017) Strength properties of bamboo and steel reinforced concrete containing manufactured sand and mineral admixtures. J King Saud Univ - Eng Sci 29:400–406. https://doi.org/10.1016/j.jksues.2016.12.003
Sathanandam T, Awoyera PO, Vijayan V, Sathishkumar K (2017) Low carbon building: experimental insight on the use of fly ash and glass fibre for making geopolymer concrete. Sustain Environ Res 27:146–153. https://doi.org/10.1016/j.serj.2017.03.005
Anandaraj S, Rooby J, Awoyera PO, Gobinath R (2019) Structural distress in glass fibre-reinforced concrete under loading and exposure to aggressive environments. Constr Build Mater 197:862–870. https://doi.org/10.1016/j.conbuildmat.2018.06.090
Komljenović M (2015) Mechanical strength and Young’s modulus of alkali-activated cement-based binders. In: Pacheco-Torgal F, Labrincha JA, Leonelli C et al (eds) Handbook of alkali-activated cements, mortars and concretes. Woodhead Publishing, Oxford, pp 171–215
Luukkonen T, Abdollahnejad Z, Yliniemi J, Kinnunen P, Illikainen M (2018) One-part alkali-activated materials: a review. Cem Concr Res 103:21–34. https://doi.org/10.1016/j.cemconres.2017.10.001
Collins F, Sanjayan JG (1999) Strength and shrinkage properties of alkali-activated slag concrete placed into a large column. Cem Concr Res 29:659–666. https://doi.org/10.1016/S0008-8846(99)00011-3
Sun Z, Lin X, Liu P, Wang D, Vollpracht A, Oeser M (2018) Study of alkali activated slag as alternative pavement binder. Constr Build Mater 186:626–634. https://doi.org/10.1016/j.conbuildmat.2018.07.154
Farhan NA, Sheikh MN, Hadi MNS (2019) Investigation of engineering properties of normal and high strength fly ash based geopolymer and alkali-activated slag concrete compared to ordinary Portland cement concrete. Constr Build Mater 196:26–42. https://doi.org/10.1016/j.conbuildmat.2018.11.083
Bilek V, Bonczková S, Hurta J, Pytlík D, Mrovec M (2017) Bond strength between reinforcing steel and different types of concrete. Procedia Eng 190:243–247. https://doi.org/10.1016/j.proeng.2017.05.333
Ding Y, Dai J-G, Shi C-J (2018) Fracture properties of alkali-activated slag and ordinary Portland cement concrete and mortar. Constr Build Mater 165:310–320. https://doi.org/10.1016/j.conbuildmat.2017.12.202
Ye H, Radlińska A (2016) Shrinkage mechanisms of alkali-activated slag. Cem Concr Res 88:126–135. https://doi.org/10.1016/j.cemconres.2016.07.001
Baščarevć Z (2015) 14 - The resistance of alkali-activated cement-based binders to chemical attack. In: Pacheco-Torgal F, Labrincha JA, Leonelli C et al (eds) Handbook of alkali-activated cements, mortars and concretes. Woodhead Publishing, Oxford, pp 373–396
Bernal SA, Rodríguez ED, de Gutiérrez RM, Provis JL (2012) Performance of alkali-activated slag mortars exposed to acids. J Sustain Cem Mater 1:138–151. https://doi.org/10.1080/21650373.2012.747235
Licht S (2017) Co-production of cement and carbon nanotubes with a carbon negative footprint. J CO2 Util 18:378–389. https://doi.org/10.1016/j.jcou.2017.02.011
Raji M, Nekhlaoui S, Hassani I-EEAE et al (2019) Utilization of volcanic amorphous aluminosilicate rocks (perlite) as alternative materials in lightweight composites. Compos Part B Eng 165:47–54. https://doi.org/10.1016/j.compositesb.2018.11.098
Shen W, Cao L, Li Q, Wen Z, Wang J, Liu Y, Dong R, Tan Y, Chen R (2016) Is magnesia cement low carbon? Life cycle carbon footprint comparing with Portland cement. J Clean Prod 131:20–27. https://doi.org/10.1016/j.jclepro.2016.05.082
Li C, Sun H, Li L (2010) A review: the comparison between alkali-activated slag (Si+Ca) and metakaolin (Si+Al) cements. Cem Concr Res 40:1341–1349. https://doi.org/10.1016/j.cemconres.2010.03.020
Liu Y, Shi C, Zhang Z, Li N (2019) An overview on the reuse of waste glasses in alkali-activated materials. Resour Conserv Recycl 144:297–309. https://doi.org/10.1016/j.resconrec.2019.02.007
Lu J-X, Poon CS (2018) Use of waste glass in alkali activated cement mortar. Constr Build Mater 160:399–407. https://doi.org/10.1016/j.conbuildmat.2017.11.080
Rakhimova NR, Rakhimov RZ (2019) Toward clean cement technologies: a review on alkali-activated fly-ash cements incorporated with supplementary materials. J Non-Cryst Solids 509:31–41. https://doi.org/10.1016/j.jnoncrysol.2019.01.025
Fernández-Jiménez A, Cristelo N, Miranda T, Palomo Á (2017) Sustainable alkali activated materials: precursor and activator derived from industrial wastes. J Clean Prod 162:1200–1209. https://doi.org/10.1016/j.jclepro.2017.06.151
Bassani M, Tefa L, Russo A, Palmero P (2019) Alkali-activation of recycled construction and demolition waste aggregate with no added binder. Constr Build Mater 205:398–413. https://doi.org/10.1016/j.conbuildmat.2019.02.031
Dembovska L, Bajare D, Ducman V, Korat L, Bumanis G (2017) The use of different by-products in the production of lightweight alkali activated building materials. Constr Build Mater 135:315–322. https://doi.org/10.1016/j.conbuildmat.2017.01.005
Sun Z, Lin X, Vollpracht A (2018) Pervious concrete made of alkali activated slag and geopolymers. Constr Build Mater 189:797–803. https://doi.org/10.1016/j.conbuildmat.2018.09.067
Puertas F, González-Fonteboa B, González-Taboada I, Alonso MM, Torres-Carrasco M, Rojo G, Martínez-Abella F (2018) Alkali-activated slag concrete: fresh and hardened behaviour. Cem Concr Compos 85:22–31. https://doi.org/10.1016/j.cemconcomp.2017.10.003
Adesanya E, Ohenoja K, Kinnunen P, Illikainen M (2017) Properties and durability of alkali-activated ladle slag. Mater Struct 50:255. https://doi.org/10.1617/s11527-017-1125-4
Thunuguntla CS, Rao TDG (2018) Effect of mix design parameters on mechanical and durability properties of alkali activated slag concrete. Constr Build Mater 193:173–188. https://doi.org/10.1016/j.conbuildmat.2018.10.189
Lee NK, Lee HK (2015) Reactivity and reaction products of alkali-activated, fly ash/slag paste. Constr Build Mater 81:303–312. https://doi.org/10.1016/j.conbuildmat.2015.02.022
Rakhimova NR, Rakhimov RZ (2018) Reaction products, structure and properties of alkali-activated metakaolin cements incorporated with supplementary materials – a review. J Mater Res Technol 8:1522–1531. https://doi.org/10.1016/j.jmrt.2018.07.006
Mithun BM, Narasimhan MC (2016) Performance of alkali activated slag concrete mixes incorporating copper slag as fine aggregate. J Clean Prod 112:837–844. https://doi.org/10.1016/j.jclepro.2015.06.026
Shi C (1996) Strength, pore structure and permeability of alkali-activated slag mortars. Cem Concr Res 26:1789–1799. https://doi.org/10.1016/S0008-8846(96)00174-3
Bernal SA, de Gutiérrez RM, Pedraza AL et al (2011) Effect of binder content on the performance of alkali-activated slag concretes. Cem Concr Res 41:1–8. https://doi.org/10.1016/j.cemconres.2010.08.017
Ismail I, Bernal SA, Provis JL, San Nicolas R, Brice DG, Kilcullen AR, Hamdan S, van Deventer JSJ (2013) Influence of fly ash on the water and chloride permeability of alkali-activated slag mortars and concretes. Constr Build Mater 48:1187–1201. https://doi.org/10.1016/j.conbuildmat.2013.07.106
Zhang Z, Yao X, Zhu H (2010) Potential application of geopolymers as protection coatings for marine concrete I. basic properties. Appl Clay Sci 49:1–6
Behfarnia K, Rostami M (2018) The effect of alkaline solution-to-slag ratio on permeability of alkali activated slag concrete. Int J Civ Eng 16:897–904. https://doi.org/10.1007/s40999-017-0234-3
Rodríguez E, Bernal S, Puertas F, Mejía de Gutiérrez R (2008) Alternative concrete based on alkali-activated slag. Mater Constr 58
Rostami M, Behfarnia K (2017) The effect of silica fume on durability of alkali activated slag concrete. Constr Build Mater 134:262–268. https://doi.org/10.1016/j.conbuildmat.2016.12.072
Bakharev T, Sanjayan JG, Cheng Y-B (2002) Sulfate attack on alkali-activated slag concrete. Cem Concr Res 32:211–216. https://doi.org/10.1016/S0008-8846(01)00659-7
Komljenović M, Baščarević Z, Marjanović N, Nikolić V (2013) External sulfate attack on alkali-activated slag. Constr Build Mater 49:31–39. https://doi.org/10.1016/j.conbuildmat.2013.08.013
Bondar D, Lynsdale CJ, Milestone NB, Hassani N (2015) Sulfate resistance of alkali activated Pozzolans. Int J Concr Struct Mater 9:145–158. https://doi.org/10.1007/s40069-014-0093-0
Tosun-Felekoğlu K (2012) The effect of C3A content on sulfate durability of Portland limestone cement mortars. Constr Build Mater 36:437–447. https://doi.org/10.1016/j.conbuildmat.2012.04.091
Xuequan W, Sheng Y, Xiaodong S, Mingshu T, Liji Y (1991) Alkali-activated slag cement based radioactive waste forms. Cem Concr Res 21:16–20. https://doi.org/10.1016/0008-8846(91)90026-E
Heikal M, Nassar MY, El-Sayed G, Ibrahim SM (2014) Physico-chemical, mechanical, microstructure and durability characteristics of alkali activated Egyptian slag. Constr Build Mater 69:60–72. https://doi.org/10.1016/j.conbuildmat.2014.07.026
Mostofinejad D, Nosouhian F, Nazari-Monfared H (2016) Influence of magnesium sulphate concentration on durability of concrete containing micro-silica, slag and limestone powder using durability index. Constr Build Mater 117:107–120. https://doi.org/10.1016/j.conbuildmat.2016.04.091
Gopalakrishnan R, Chinnaraju K (2019) Durability of ambient cured alumina silicate concrete based on slag/fly ash blends against sulfate environment. Constr Build Mater 204:70–83. https://doi.org/10.1016/j.conbuildmat.2019.01.153
Bakharev T, Sanjayan JG, Cheng Y-B (2001) Resistance of alkali-activated slag concrete to carbonation. Cem Concr Res 31:1277–1283. https://doi.org/10.1016/S0008-8846(01)00574-9
Fernández-Jiménez A, Puertas F (2001) Setting of alkali-activated slag cement. Influence of activator nature. Adv Cem Res 13:115–121. https://doi.org/10.1680/adcr.2001.13.3.115
Chatterji S (2005) Chemistry of alkali–silica reaction and testing of aggregates. Cem Concr Compos 27:788–795. https://doi.org/10.1016/j.cemconcomp.2005.03.005
Bakharev T, Sanjayan JG, Cheng Y-B (2000) Effect of admixtures on properties of alkali-activated slag concrete. Cem Concr Res 30:1367–1374. https://doi.org/10.1016/S0008-8846(00)00349-5
CHENGNING W (1993) Properties and applications of alkali-slag cement. J Chin Ceram Soc 21:176–181
Elfmarkova V, Spiesz P, Brouwers HJH (2015) Determination of the chloride diffusion coefficient in blended cement mortars. Cem Concr Res 78:190–199. https://doi.org/10.1016/j.cemconres.2015.06.014
Yuan Q, Shi C, Schutter GD et al (2009) Chloride binding of cement-based materials subjected to external chloride environment – a review. Constr Build Mater 23:1–13. https://doi.org/10.1016/j.conbuildmat.2008.02.004
Dhir RK, El-Mohr MAK, Dyer TD (1996) Chloride binding in GGBS concrete. Cem Concr Res 26:1767–1773. https://doi.org/10.1016/S0008-8846(96)00180-9
ASTM C1202 (2017) Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration, ASTM International, West Conshohocken, PA, 2019, www.astm.org. Accessed 5 Feb 2019
Fernandez-Jimenez A, García-Lodeiro I, Palomo A (2007) Durability of alkali-activated fly ash cementitious materials. J Mater Sci 42:3055–3065. https://doi.org/10.1007/s10853-006-0584-8
Zhu H, Zhang Z, Zhu Y, Tian L (2014) Durability of alkali-activated fly ash concrete: chloride penetration in pastes and mortars. Constr Build Mater 65:51–59. https://doi.org/10.1016/j.conbuildmat.2014.04.110
Park J, Ann K, Cho C (2015) Resistance of Alkali-Activated Slag Concrete to Chloride-Induced Corrosion. Adv Mater Sci Eng, 2015, 7 pages. https://doi.org/10.1155/2015/273101
Shi C, Roy D, Krivenko P (2003) Alkali-activated cements and concretes. CRC Press, London
Mohammed M (2015) Multi-scale response of sustainable self-compacting concrete (SCC) to carbonation and chloride penetration. PhD thesis, Univ Nottingham
He J, Gao Q, Wu Y, He J, Pu X (2018) Study on improvement of carbonation resistance of alkali-activated slag concrete. Constr Build Mater 176:60–67. https://doi.org/10.1016/j.conbuildmat.2018.04.117
Badar MS, Kupwade-Patil K, Bernal SA et al (2014) Corrosion of steel bars induced by accelerated carbonation in low and high calcium fly ash geopolymer concretes. Constr Build Mater 61:79–89. https://doi.org/10.1016/j.conbuildmat.2014.03.015
Provis JL, Bernal SA (2014) Geopolymers and related alkali-activated materials. Annu Rev Mater Res 44:299–327. https://doi.org/10.1146/annurev-matsci-070813-113515
Ke X, Bernal SA, Provis JL (2016) Controlling the reaction kinetics of sodium carbonate-activated slag cements using calcined layered double hydroxides. Cem Concr Res 81:24–37. https://doi.org/10.1016/j.cemconres.2015.11.012
Palacios M, Puertas F (2006) Effect of carbonation on alkali-activated slag paste. J Am Ceram Soc 89:3211–3221. https://doi.org/10.1111/j.1551-2916.2006.01214.x
Zhang X, Wang L, Zhang J, Liu Y (2017) Corrosion-induced flexural behavior degradation of locally ungrouted post-tensioned concrete beams. Constr Build Mater 134:7–17. https://doi.org/10.1016/j.conbuildmat.2016.12.140
Monticelli C, Natali ME, Balbo A, Chiavari C, Zanotto F, Manzi S, Bignozzi MC (2016) A study on the corrosion of reinforcing bars in alkali-activated fly ash mortars under wet and dry exposures to chloride solutions. Cem Concr Res 87:53–63. https://doi.org/10.1016/j.cemconres.2016.05.010
Ceukelaire LD, Nieuwenburg DV (1993) Accelerated carbonation of a blast-furnace cement concrete. Cem Concr Res 23:442–452. https://doi.org/10.1016/0008-8846(93)90109-M
Ma Z, Zhu F, Ba G (2019) Effects of freeze-thaw damage on the bond behavior of concrete and enhancing measures. Constr Build Mater 196:375–385. https://doi.org/10.1016/j.conbuildmat.2018.11.041
Pacheco-Torgal F, Abdollahnejad Z, Camões AF, Jamshidi M, Ding Y (2012) Durability of alkali-activated binders: a clear advantage over Portland cement or an unproven issue? Constr Build Mater 30:400–405. https://doi.org/10.1016/j.conbuildmat.2011.12.017
Shahrajabian F, Behfarnia K (2018) The effects of nano particles on freeze and thaw resistance of alkali-activated slag concrete. Constr Build Mater 176:172–178. https://doi.org/10.1016/j.conbuildmat.2018.05.033
Tan H, Deng X, He X, Zhang J, Zhang X, Su Y, Yang J (2019) Compressive strength and hydration process of wet-grinded granulated blast-furnace slag activated by sodium sulfate and sodium carbonate. Cem Concr Compos 97:387–398. https://doi.org/10.1016/j.cemconcomp.2019.01.012
Thahira Banu S, Chitra G, Awoyera P, Gobinath R Structural retrofitting of corroded fly ash based concrete beams with fibres to improve bending characteristics. Aust J Struct Eng, (in press)
Yuan Y, Ji Y, Jiang J (2009) Effect of corrosion layer of steel bar in concrete on time-variant corrosion rate. Mater Struct 42:1443–1450. https://doi.org/10.1617/s11527-008-9464-9
Thahira Banu S, Chitra G, Gobinath R et al (2018) Sustainable structural retrofitting of corroded concrete using basalt fibre composite. Ecol Environ Conserv 24:1384–1388
Ravikumar D, Neithalath N (2013) Electrically induced chloride ion transport in alkali activated slag concretes and the influence of microstructure. Cem Concr Res 47:31–42. https://doi.org/10.1016/j.cemconres.2013.01.007
Babaee M, Castel A (2018) Chloride diffusivity, chloride threshold, and corrosion initiation in reinforced alkali-activated mortars: role of calcium, alkali, and silicate content. Cem Concr Res 111:56–71. https://doi.org/10.1016/j.cemconres.2018.06.009
Criado M (2015) 13 - the corrosion behaviour of reinforced steel embedded in alkali-activated mortar. In: Pacheco-Torgal F, Labrincha JA, Leonelli C et al (eds) Handbook of alkali-activated cements, mortars and concretes. Woodhead Publishing, Oxford, pp 333–372
Liu J-C, Tan KH, Yao Y (2018) A new perspective on nature of fire-induced spalling in concrete. Constr Build Mater 184:581–590. https://doi.org/10.1016/j.conbuildmat.2018.06.204
Awoyera P (2014) Forensic investigation of fire-affected concrete buildings. LAP LAMBERT Academic Publishing
Awoyera P, Arum C, Akinwumi I (2014) Significance of concrete cover to reinforcement in structural element at varying temperatures. Int J Sci Eng Res 5:1120–1123
Viswanathan V, Laha T, Balani K, Agarwal A, Seal S (2006) Challenges and advances in nanocomposite processing techniques. Mater Sci Eng R Rep 54:121–285. https://doi.org/10.1016/j.mser.2006.11.002
Türker HT, Balçikanli M, Durmuş İH, Özbay E, Erdemir M (2016) Microstructural alteration of alkali activated slag mortars depend on exposed high temperature level. Constr Build Mater 104:169–180. https://doi.org/10.1016/j.conbuildmat.2015.12.070
Panias D, Balomenos E, Sakkas K (2015) 16 - the fire resistance of alkali-activated cement-basedconcrete binders. In: Pacheco-Torgal F, Labrincha JA, Leonelli C et al (eds) Handbook of alkali-activated cements, mortars and concretes. Woodhead Publishing, Oxford, pp 423–461
Li Y-L, Zhao X-L, Raman RKS, Al-Saadi S (2018) Thermal and mechanical properties of alkali-activated slag paste, mortar and concrete utilising seawater and sea sand. Constr Build Mater 159:704–724. https://doi.org/10.1016/j.conbuildmat.2017.10.104
Wang S-D, Pu X-C, Scrivener KL, Pratt PL (1995) Alkali-activated slag cement and concrete: a review of properties and problems. Adv Cem Res 7:93–102. https://doi.org/10.1680/adcr.1995.7.27.93
Provis J, Van Deventer J (2014) Alkali activated materials : state-of-the-art report, RILEM TC 224-AAM. New York London
Monkman S, MacDonald M (2017) On carbon dioxide utilization as a means to improve the sustainability of ready-mixed concrete. J Clean Prod 167:365–375. https://doi.org/10.1016/j.jclepro.2017.08.194
Stafford FN, Dias AC, Arroja L, Labrincha JA, Hotza D (2016) Life cycle assessment of the production of Portland cement: a southern Europe case study. J Clean Prod 126:159–165. https://doi.org/10.1016/j.jclepro.2016.02.110
Ishak SA, Hashim H (2015) Low carbon measures for cement plant – a review. J Clean Prod 103:260–274. https://doi.org/10.1016/j.jclepro.2014.11.003
Awoyera PO, Okoro UC (2019) Filler-ability of highly active Metakaolin for improving morphology and strength characteristics of recycled aggregate concrete. Silicon. https://doi.org/10.1007/s12633-018-0017-8
Author information
Authors and Affiliations
Corresponding author
Additional information
Publisher’s Note
Springer Nature remains neutral with regard to jurisdictional claims in published maps and institutional affiliations.
Rights and permissions
About this article
Cite this article
Awoyera, P., Adesina, A. Durability Properties of Alkali Activated Slag Composites: Short Overview. Silicon 12, 987–996 (2020). https://doi.org/10.1007/s12633-019-00199-1
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s12633-019-00199-1