Abstract
Compressive stress due to intermetallic (IMC) growth appears to be the main driving force for whisker formation, but many of the underlying mechanisms relating the IMC to stress and whisker formation are not understood. To better understand these fundamental processes, we have measured IMC, stress and whisker evolution in Sn layers deposited on Cu. We present systematic results of the effect of changing the Sn layer structure by modifying the grain size, thickness, Pb content, microstructure, and IMC morphology/growth kinetics. We have also made corresponding measurements of the mechanical properties of the Sn with similar changes in the structure and composition without the growth of IMC. We show that modifications that enhance the stress relaxation in the Sn also lead to reduced whisker growth.
Article PDF
Similar content being viewed by others
Avoid common mistakes on your manuscript.
References
J.A. Brusse et al., in Proc. 22 nd Capacitor and Resistor Technology Symposium (2002), pp. 67–80.
G.T. Galyon, IEEE Trans. Electron. Pkg. Manu., 28 (2005), pp. 94–122.
NASA, Multiple Examples of Whisker-induced Failures are Documented on the NASA Website, nepp.nasa.gov/whisker/.
S.M. Arnold, IEEE Electron. Comp. Technol. Conf. (1959), pp. 75–82.
K.N. Tu and R.D. Thompson, Acta Metall., 30 (1982), pp. 947–952.
J. Smetana, IEEE Trans. Electron. Pkg. Manu., 30 (2007), pp. 11–22.
B.Z. Lee and D.N. Lee, Acta Mater., 46 (1998), pp. 3701–3714.
N. Jadhav et al., IEEE Trans. Electron. Pkg. Manu., 33 (2010), pp. 183–192.
N. Jadhav et al., J. Electron. Mater. (accepted 2011).
N. Jadhav et al., JOM, 62(7) (2010), pp. 30–37.
P. Oberndorff et al., “Intermetallic Formation in Relation to Tin Whiskers” (Paper presented at the IPC/Soldertec International Conference on Lead-Free Electronics, Brussels, 2003).
W. Zhang et al., IEEE Trans. Electron. Pkg. Manu., 28 (2005), pp. 85–93.
E. Chason and J.A. Floro, MRS Symposium Proceedings VI (Pittsburgh, PA: MRS, 1997), pp. 417–422.
L.B. Freund and S. Suresh, Thin Film Materials: Stress, Defect Formation and Surface Evolution, 1st ed. (Cambridge, U.K.: Cambridge University Press, 2009), pp. 86–93.
E. Chason et al., Appl. Phys. Lett., 92 (2008), p. 171901.
J.W. Shin and E. Chason, J. Mater. Res., 24 (2009), pp. 1522–1528.
M. Onishi and H. Fujibuchi, Trans. Jpn. Inst. Metals, 16 (1975), pp. 539–547.
E. Buchovecky et al., J. Electron. Mater., 38 (2009), pp. 2676–2684.
Y. Choi and S. Suresh, Acta Mater., 50 (2002), pp. 1881–1893.
R.-M. Kelle et al., J. Mater. Res., 13 (1998), pp. 1307–1317.
W.J. Boettinger et al., Acta Mater., 53 (2005), pp. 5033–5050.
C.-F. Yu et al., Microelectronics Reliability, 50 (2010), pp. 1146–1151.
Y. Zhang et al., Proc. IPC SMEMA Council Apex (Blackburn, IL: IPC-Association Connecting Electronics Industries, 2002), pp. S06-1–8.
E. Sandnes et al., J. Electron. Mater., 37 (2008), pp. 490–497.
A. Rae and C.A. Handwerker, Circuits Assembly, 15 (2004), pp. 20–25.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Chason, E., Jadhav, N. & Pei, F. Effect of layer properties on stress evolution, intermetallic volume, and density during tin whisker formation. JOM 63, 62–68 (2011). https://doi.org/10.1007/s11837-011-0178-z
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11837-011-0178-z