Conclusions
Nitriding of austenitic steel of the 12Kh18N10T type can be speeded up by using ordinary furnaces. The main condition for increasing the rate of the process is to ensure the proper flow of the saturating gas around the machine part, which can be achieved by using a deflector.
Article PDF
Avoid common mistakes on your manuscript.
Additional information
Translated from Metallovedenie i Termicheskaya Obrabotka Metallov, No. 7, pp. 42–43, July, 1978.
Rights and permissions
About this article
Cite this article
Tokarev, Y.G., Lin, S.T. Acceleration of nitriding of steel 12Kh18N10T. Met Sci Heat Treat 20, 560–561 (1978). https://doi.org/10.1007/BF00780335