Abstract
The welding of thick high strength aluminum alloy plate was exceedingly difficult. Traditional arc welding was prone to softening the welded joints and involves multilayer; meanwhile, multi-pass welding may cause great residual welding stress, and deformation resulted in dampening the wide expansion of the welding structure of thick high strength aluminum alloy plates. Therefore, it was urgent to develop advanced materials and welding technologies to enhance the comprehensive mechanical properties of welded joints. Fiber laser boasted the advantages such as perfect monochromaticity and high quality light beam. In order to decrease the thermal loss of the welding heat source on the matrix, small power fiber laser and super narrow gap groove were applied for the effective welding of the 20-mm thick 7A52 aluminum alloy. The welding adopted multilayer and single pass welding with the groove width no wider than 4 mm. The weld was composed of four layers and the size was no wider than 4.5 mm, which was basically consistent with the widths of the whole. The parent metal was welded with 5183 alloy and 5E06 alloy. Fiber optical microscope, scanning electron microscope (SEM), transmission electron microscope (TEM), and tensile testing machine were employed to investigate the influence of Er-Zr microalloying aluminum alloy welding wires upon the microstructure and mechanical properties of the welded joints.
Article PDF
Similar content being viewed by others
Avoid common mistakes on your manuscript.
References
Wu YF, Kim GY, Russell AM (2012) Effects of mechanical alloying on an AL6061-CNT composite fabricated by semi-solid power processing. Mater Sci Eng A 48:164–172
Chen CS, Yang JG, Tan AH (2009) Study of welding peak temperatures on microstructures and hardness of heat affected zone in 2024-T3 aluminium alloy. Mater Sci Technol 25:896–904
Hu B, Richardson IM (2007) Microstructure and mechanical properties of AA7075(T6) hybrid laser/GMA welds. Mater Sci Eng A 459:94–100
Rhodes CG, Mahoney MW, Bingel WH (1997) Effect of friction stir welding on microstructure of 7075 aluminum. Scr Mater 36:69–75
Jones MJ, Heurtier P, Desrayaud C (2005) Correlation between microstructure and microhardness in a friction stir welded 2024 aluminium alloy. Scr Mater 52:693–697
Sullivan A, Robson JD (2008) Microstructural properties of friction stir welded and post-weld heat-treated 7449 aluminium alloy thick plate. Mater Sci Eng A 478:351–360
Cavaliere P, Cerri E, Squillace A (2005) Mechanical response of 2024-7075 aluminium alloys joined by friction stir welding. J Mater Sci 40:3669–3676
Amancio-Filho ST, Sheikhi S, Dos-Santos JF, Bolfarini C (2008) Preliminary study on the microstructure and mechanical properties of dissimilar friction stir welds in aircraft aluminium alloys 2024-T351 and 6056-T4. J Mater Process Technol 206:132–142
Wei ST, Hao CY, Chen JC (2007) Study of frition stir welding of 1420 aluminum-lithium alloy. Mater Sci Eng A Struct 452:170–177
Koteswara SR, Madhusudhana RG, Srinivasa RK (2005) Reasons for superior mechanical and corrosion properties of 2219 aluminum alloy electron beam welds. Mater Charact 40:236–248
Zhang C, Li G, Gao M, Yan J, Zeng XY (2013) Microstructure and process characterization of laser-cold metal transfer hybrid welding of AA6061 aluminum alloy. Int J Adv Manuf Technol 68:1253–1260
Balasubramanian V, Ravisankar V, Madhusudhan Reddy G (2008) Influences of pulsed current welding and post weld aging treatment on fatigue crack growth behaviour of AA7075 aluminium alloy joints. Int J Fatigue 30:405–416
Yu YC, Wang CM, Hu XY (2010) Porosity in fiber laser formation of 5A06 aluminum alloy. J Mech Sci Technol 24:1077–1082
Shi H, Zhang K, Xu ZY, Huang TY, Fan LW, Bao WN (2014) Applying statistical models optimize the process of multi-pass narrow-gap laser welding with filler wire. Int J Adv Manuf Technol 75:279–291
Yu YC, Yang SL, Yin Y (2013) Multi-pass laser welding of thick plate with filler wire by using a narrow gap joint configuration. J Mech Sci Technol 27:2125–2131
Singh V, Prasad KS, Gokhale AA (2004) Effect of minor Sc additions on structure, age hardening and tensile properties of aluminium alloy AA8090 plate. Scr Mater 50:903–908
Fuller CB, Krause AR, Dunand DC M (2002) Microstructure and mechanical properties of a 5754 aluminum alloy modified by Sc and Zr additions. Sci Eng A 338:8–16
Norman AF, Hyde K, Costello F (2003) Examination of the effect of Sc on 2000 and 7000 series aluminium alloy castings: for improvements in fusion welding. Mater Sci Eng A 354:188–198
Halevy OI, Beeri JH (2012) Sc-strengthened commercial purity aluminum under high pressure. Mater Sci 45:589–592
Costa S, Puga H, Barbosa J, Pinto MP (2012) The effect of Sc additions on the microstructure and age hardening behaviour of as cast Al-Sc alloys. Mater Des 42:347–352
Lefebvre W, Danoix F, Hallem H (2009) Precipitation kinetic of Al3(Sc, Zr) dispersoids in aluminium. J Alloys Compds Compd 470:107–110
Xing PF, Gao B, Zhuang YX, Liu KH, Tu GF (2010) On the modification of hypereutectic Al-Si alloys using rear earth Er. Acta Metall Sin 23:327–333
Wen SP, Xing ZB, Huang H (2009) The effect of erbium on the microstructure and mechanical properties of Al-Mg-Mn-Zr alloy. Mater Sci Eng A 516:42–49
Nie ZR, Li BL, Wang W (2002) Research on rare earth in aluminum. Mater Sci Forum 402:1731–1736
Satoh BK, Toyoda M (1975) Joint strength of heavy plates with lower strength weld metal. Weld J 54:311–319
Nowak D, Feng G, Jones M, Erikson C (2004) Laser hot-wire welding for minimizing defects. ICALEO
Onishi T, Mizutani M, Kawahito Y, Katayama S (2009) High-power fiber laser butt welding of thick high-strength steel plate using sensing system with hot wire. ICALEO
Dittrich D, Schedewy R, Brenner B, Standfuß J (2013) Laser-multi-pass-narrow-gap-welding of hot crack sensitive thick aluminum plates. Phys Procedia 41:225–233
Chen K, Xiao RS, Zuo TC, Ji Q (2005) Laser welding of Al-Mg alloy with the thin plate. Proc SPIE 5629:155–160
Katayama S, Iviizutanf M, Matsunawa A (2003) Development of porosity prevention procedures during laser welding. Proc SPIE 4831:281–288
Turnbull D (1950) Formation of crystal nuclei in liquid metals. J Appl Phys 21:1022–1028
Witzke S, Riquet JP (1982) Columnar-equiaxed transition in Al-Cu alloy ingots. Acta Metall 30:1717–1722
Duggan G, Tong M, Browne DJ (2015) Modelling the creation and destruction of columnar and equiaxed zones during solidification and melting in multi-pass welding of steel. Comput Mater Sci 97:285–294
Li HY, Gao ZH, Yin H, Jiang HF, Su XJ, Bin J (2013) Effects of Er and Zr additions on precipitation and recrystallizaton of pure aluminum. Scr Mater 68:59–62
Yang DX, Li XY, He DY, Huang H (2013) Effect of minor Er and Zr on microstructure and mechanical properties of Al–Mg–Mn alloy (5083) welded joints. Mater Sci Eng A 561:226–231
Wen SP, Gao KY, Li Y, Huang H, Nie ZR (2013) Effect of gap on plasma and molten pool dynamics during laser lap welding for T-joints. Int J Adv Manuf Technol 69:1105–1112
Jandaghi M, Parvin P, Torkamany MJ, Sabbaghzadeh J (2009) Measurement of the composition change in Al5754 alloy during long pulsed Nd:YAG laser welding based on LIBS. J Phys D Appl Phys 42:205301.1–205301.8
Lefebvre F, Ganguly S, Sinclair I (2005) Micromechanical aspects of fatigue in a MIG welded aluminium airframe alloy. Mater Sci Eng A 397:338–345
Zhao H, Debroy T (2001) Weld metal composition Chang during conduction mode laser welding of aluminum alloy 5182. Metall Mater Trans B 32:163–172
Dilthey U, Goumeniouk A, Lopota V (2001) Development of a theory for alloying element losses during laser beam welding. J Phys D Appl Phys 34:81–86
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Zhang, Z.H., Dong, S.Y., Wang, Y.J. et al. Study on microstructures and mechanical properties of super narrow gap joints of thick and high strength aluminum alloy plates welded by fiber laser. Int J Adv Manuf Technol 82, 99–109 (2016). https://doi.org/10.1007/s00170-015-7334-5
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s00170-015-7334-5